Parts Shot peening process
Parts Shot peening process
(1) The individual parts can also be carried out on the assembly Shot peening.
(2) The drawings indicate non-Shot peening parts, should take measures to shield.
(3) on a regular basis (every 4 hours or per shift) Shot peening strength test, ensure the stability of the process parameters.
(4) Periodic inspection Gangwangangsha quality.
(5) Shot peening intensity tolerance range can be set from 0 to + 30% of the arc height.
(6) In the inspection found below the specified test piece Shot peening intensity, the batch production of parts can be re-fill spray again.